| dc.description | A numerical integration scheme is presented for integration of the pressure-sensitive yield criterion due to Gurson, suitable for explicit dynamic finite element calculations. This scheme utilizes a sub-increment approach to Mayntain stability for the large strain increments and intense triaxiality that can occur under high strain rate loading. A number of validation problems are presented after which two laboratory-scale high strain experiments are simulated. The integration scheme is shown to be stable and to capture the onset of tensile fracture under high strain rate loading conditions. |
| Формат | application.pdf |
| Издатель | EDP Sciences |
| Копирайт | © EDP Sciences, 1998 |
| Название | Numerical simulation of ductile fracture during high strain rate deformation |
| Тип | research-article |
| DOI | 10.1051/epjap:1998269 |
| Electronic ISSN | 1286-0050 |
| Print ISSN | 1286-0042 |
| Журнал | The European Physical Journal Applied Physics |
| Том | 4 |
| Первая страница | 257 |
| Последняя страница | 267 |
| Аффилиация | Worswick M. J.; Department of Mechanical Engineering, University of Waterloo Waterloo, Ontario, Canada N2L 3G1 |
| Аффилиация | Pelletier P.; SNC Industrial Technologies Ltd. 5 Montée des Arsenaux Le Gardeur, Québec, Canada J5Z 2P4 |
| Выпуск | 3 |